前言:EMC130C,高可靠性 阻燃性 ,日本东洋纺织,PBT /PET,家电部件
| 日本东洋纺 PBT VYLOPET EMC341技术参数 |
| 性能项目 | 试验条件 | 测试方法 | 测试数据 |
| 比重 |
| ASTMD792 | 1.63 | g/cm3 |
| 收缩率-流动(3.00mm) |
| ASTMD955 | 0.300.90 | % |
| 吸水率(24hr) |
| ASTMD570 | 0.050 | % |
| 洛氏硬度(M级) |
| ASTMD785 | 95 |
|
| 抗张强度(屈服) |
| ASTMD638 | 155 | MPa |
| 伸长率(断裂) |
| ASTMD638 | 1.9 | % |
| 弯曲模量 |
| ASTMD790 | 12000 | MPa |
| 弯曲强度(屈服) |
| ASTMD790 | 220 | MPa |
| 悬壁梁缺口冲击强度 |
| ASTMD256 | 90 | J/m |
| 载荷下热变形温度 | 0.45MPa,未退火 | ASTMD648 | 245 | °C |
| 载荷下热变形温度 | 1.8MPa,未退火 | ASTMD648 | 235 | °C |
| 熔融温度 |
| DSC | 255 | °C |
| 线形热膨胀系数-流动 |
| ASTMD696 | 2.5E-5 | cm/cm/°C |
| RTIElec |
| UL746 | 130 | °C |
| RTIImp |
| UL746 | 130 | °C |
| RTI |
| UL746 | 130 | °C |
| 体积电阻率 |
| ASTMD257 | 1.0E 18 | ohmscm |
| 介电强度(2.00mm) |
| ASTMD149 | 25 | kV/mm |
| 耐电弧性 |
| ASTMD495 | 130 | sec |
| UL阻燃等级 |
| UL94 | HB |
|